受BTA保护的白铜在模拟工业大气环境中的腐蚀行为
|
|
Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere
|
|
图4. 在不同腐蚀周期下BTA处理前后白铜的极化曲线 |
Fig.4. Polarization curves of copper-nickel alloys before (a) and after (b) BTA treatment as function of corrosion time (E—corrosion potential, i—corrosion current density) |
![]() |