受BTA保护的白铜在模拟工业大气环境中的腐蚀行为
黄松鹏1,2, 彭灿1,2, 曹公望1,2, 王振尧1,2()
Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere
HUANG Songpeng1,2, PENG Can1,2, CAO Gongwang1,2, WANG Zhenyao1,2()

图3. 在不同腐蚀周期下BTA处理前后白铜的腐蚀速率曲线和相应的腐蚀表面形貌

Fig.3. Corrosion rate curves and surface morphologies (insets) of copper-nickel alloys before and after BTA treatment in different corrosion time (t)