Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water
TAN Jibo, WANG Xiang, WU Xinqiang(), HAN En-Hou

图12. 316LN不锈钢在高温高压水环境中距离裂纹源不同位置处的疲劳裂纹扩展速率

Fig.12. The fatigue crack growth rate (da/dN) at different distances to crack initiation sites for 316LN stainless steel in high-temperature pressurized water