316LN不锈钢管状试样高温高压水的腐蚀疲劳行为
|
|
Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water
|
|
图11. 316LN不锈钢管状试样(0.004 × 10-2 s-1)内表面二次裂纹以及氧化物 |
Fig.11. Morphology of secondary cracks (a) and oxides (b) on inner surface of 316LN stainless steel hollow specimen |
![]() |