316LN不锈钢管状试样高温高压水的腐蚀疲劳行为
谭季波, 王翔, 吴欣强(), 韩恩厚
Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water
TAN Jibo, WANG Xiang, WU Xinqiang(), HAN En-Hou

图8. 不同应变速率条件下316LN不锈钢管状试样疲劳断口宏观形貌
(a) 0.4 × 10-2 s-1 (b) 0.04 × 10-2 s-1 (c) 0.004 × 10-2 s-1

Fig.8. Macromorphologies of fatigue fractures of 316LN stainless steel hollow specimens at different strain rates