316LN不锈钢管状试样高温高压水的腐蚀疲劳行为
|
|
Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water
|
|
图5. 316LN不锈钢管状试样和标准棒状试样[ |
Fig.5. Corrosion fatigue data of 316LN stainless steel hollow specimen and standard round bar specimen[ |
![]() |