316LN不锈钢管状试样高温高压水的腐蚀疲劳行为
谭季波, 王翔, 吴欣强(), 韩恩厚
Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water
TAN Jibo, WANG Xiang, WU Xinqiang(), HAN En-Hou

图1. 316LN不锈钢管状试样形状尺寸示意图

Fig.1. Schematic of shape and size of 316LN stainless steel hollow specimen (unit: mm)