W-Ni-Fe三元合金等离子球化过程的SPH仿真研究
侯玉柏1,2,3, 于月光2(), 郭志猛1
Simulation Study of Smoothed Particle Hydrodynamics (SPH) Method in Plasma Spheroidization of W-Ni-Fe Ternary Alloys
HOU Yubai1,2,3, YU Yueguang2(), GUO Zhimeng1

图7. 不同条件下液滴融合后的球化度及致密度曲线
(a) models 1-3 (b) models 4-6 (c) models 7-9 (d) models 10-12

Fig.7. The spheroidization ratio and compactness curves obtained by an interpolation method