W-Ni-Fe三元合金等离子球化过程的SPH仿真研究
侯玉柏1,2,3, 于月光2(), 郭志猛1
Simulation Study of Smoothed Particle Hydrodynamics (SPH) Method in Plasma Spheroidization of W-Ni-Fe Ternary Alloys
HOU Yubai1,2,3, YU Yueguang2(), GUO Zhimeng1

图5. W-Ni-Fe三元合金在不同W液滴直径下(模型7~9)的液滴融合状态
(a) 2.5 μm (b) 3.0 μm (c) 3.5 μm

Fig.5. Simulation results for W-Ni-Fe ternary alloy after droplet fusion under different diameters of W (models 7-9)