喷涂工艺对Ta2O5原位复合钽基纳米晶涂层微观结构及摩擦磨损性能的影响
|
|
Effect of Spraying Process on Microstructure and Tribological Properties of Ta2O5 In Situ Composite Nanocrystalline Ta-Based Coatings
|
|
图3. No.1~No.7钽基涂层表面形貌的SEM像 |
Fig.3. Surface SEM images of No.1 (a), No.2 (b), No.3 (c), No.4 (d), No.5 (e), No.6 (f), and No.7 (g) Ta-based coatings |
![]() |