喷涂工艺对Ta2O5原位复合钽基纳米晶涂层微观结构及摩擦磨损性能的影响
|
|
Effect of Spraying Process on Microstructure and Tribological Properties of Ta2O5 In Situ Composite Nanocrystalline Ta-Based Coatings
|
|
图2. 钽基涂层的XRD谱 |
Fig.2. XRD spectrum of Ta-based coating |
![]() |