18.7Cr-1.0Ni-5.8Mn-0.2N节Ni型双相不锈钢的大变形热压缩软化行为
|
|
Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain
|
|
图9. 双相不锈钢试样在0.1 s-1变形条件下的反极图 |
Fig.9. The inverse pole figures (IPFs) of duplex stainless steel samples deformed at 0.1 s-1 and 1123-1423 K |
![]() |