18.7Cr-1.0Ni-5.8Mn-0.2N节Ni型双相不锈钢的大变形热压缩软化行为
|
|
Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain
|
|
图2. 双相不锈钢试样在1123~1423 K、0.01~10 s-1变形时的真应力-真应变曲线 |
Fig.2. True stress-true strain curves of duplex stainless steel samples deformed at 1123-1423 K ( |
![]() |