热力耦合对一种第四代镍基单晶高温合金1100℃蠕变组织演变的影响
|
|
Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC
|
|
图5. 镍基单晶高温合金在1100℃、不同应力状态下蠕变200 h横截面枝晶干的显微组织 |
Fig.5. SEM images of dendrite region at cross sections of the nickel-based single-crystal superalloy after creep for 200 h at 1100oC and various stresses |
![]() |