热力耦合对一种第四代镍基单晶高温合金1100℃蠕变组织演变的影响
|
|
Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC
|
|
图1. 变截面蠕变试样尺寸示意图 |
Fig.1. Schematic of the variable section creep (VSC) specimens (unit: mm) |
![]() |