选区激光熔化René 88DT高温合金的晶粒组织及冶金缺陷调控
|
|
Grain Structure and Metallurgical Defects Regulation of Selective Laser Melted René 88DT Superalloy
|
|
图3. 选区激光熔化René 88DT高温合金试样的缺陷形貌 |
Fig.3. Defect morphologies of selective laser melted René 88DT specimens |
![]() |