综述:活性元素作用机理——氧化物“钉扎”模型
|
|
Review: Mechanism of Reactive Element Effect—Oxide Pegging
|
|
图2. 裂纹通过氧化物栓时可能选择的路径(I, II或 III)[ |
Fig.2. Schematic diagram of different routes (I, II or III) of interface crack propagation an oxide peg[ |
![]() |