耐热铝基合金研究进展:微观组织设计与析出策略
高一涵, 刘刚(), 孙军()
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
GAO Yihan, LIU Gang(), SUN Jun()

图13. 一种Ag微合金化的Al-Mg-Si合金中G.P.区、β''以及β'相内Ag分布随时效过程的演化规律[57]

Fig.13. Evolution of Ag distribution in G.P. zone, β'' and β' precipitates in an Ag-microalloyed Al-Mg-Si alloy during ageing process (a~d)[57]