耐热铝基合金研究进展:微观组织设计与析出策略
|
|
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
|
|
图8. 具有核-壳结构的Al3(Sc, Zr, Er)基析出相的APT照片,及数种Al-Sc-Zr-Er基合金在300和400℃的抗蠕变性能[ |
Fig.8. Representative atom probe tomography (APT) images showing the Al3(Sc,Zr,Er)-based nanoprecipitates with core-shell structure (a~d)[ |
![]() |