耐热铝基合金研究进展:微观组织设计与析出策略
|
|
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
|
|
图7. Al-Ni基与Al-Ce基合金的共晶相形貌及相应的高温力学性能[ |
Fig.7. Eutectic phases (a, c) and high-temperature mechanical properties (b, d) in Al-Ni-bsed (a, b)[ |
![]() |