耐热铝基合金研究进展:微观组织设计与析出策略
|
|
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
|
|
图6. 一种快速凝固制备的A356合金中的纳米层级结构,包含α-Al基体中的Si纳米颗粒以及共晶Si中的Al纳米颗粒[ |
Fig.6. Nanostructural hierarchy in a rapid solidification (RS) A356 alloy, containing Si nanoprecipitates highly dispersed in α-Al matrix (a, b) as well as nanoscale Al particles embedded in eutectic Si (c)[ |
![]() |