耐热铝基合金研究进展:微观组织设计与析出策略
|
|
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
|
|
图4. 典型的Al-Cu与Al-Sc二元平衡相图,及高温下常见合金化元素在Al基体中的扩散速率汇总[ |
Fig.4. Representative equilibrium binary phase diagram of Al-Cu (a)[ |
![]() |