耐热铝基合金研究进展:微观组织设计与析出策略
|
|
Recent Progress in High-Temperature Resistant Aluminum-Based Alloys: Microstructural Design and Precipitation Strategy
|
|
图2. Al-TM基材料的典型纳米晶结构与第二相颗粒[ |
Fig.2. Representative nanocrystalline structure (a) and second-phase particles (b) in Al-TM-based alloys[ |
![]() |