加工硬化和退火软化效应对316不锈钢厚壁管-管对接接头残余应力计算精度的影响 |
| 李索, 陈维奇, 胡龙, 邓德安 |
|
Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint |
| LI Suo, CHEN Weiqi, HU Long, DENG Dean |
| 图5 316LN不锈钢室温循环应力-应变曲线的计算结果与实验数据[ |
| Fig.5 Comparisons of the predicted cyclic stress-strain curves with the experimental data[ |
|