核电安全端结构中材料拘束的作用范围 |
| 戴悦, 杨杰, 陈浩峰 |
|
Effect Range of Material Constraint in Nuclear Safe End Structure |
| DAI Yue, YANG Jie, CHEN Haofeng |
| 图12 52Mb宽度为100和200 mm时核电安全端实际结构与简化结构FAD的对比 (a) W52Mb = 100 mm (b) W52Mb = 200 mm |
| Fig.12 Comparisons of FAD between actual and simplified nuclear safe end structure |
|