核电安全端结构中材料拘束的作用范围 |
| 戴悦, 杨杰, 陈浩峰 |
|
Effect Range of Material Constraint in Nuclear Safe End Structure |
| DAI Yue, YANG Jie, CHEN Haofeng |
| 图6 核电安全端实际结构在不同材料拘束下的失效评定图(FAD) |
| Fig.6 Failure assessment diagram (FAD) of actual nuclear safe end structure under different material constraints (Kr—dimensionless stress intensity factor, Lr—dimensionless load factor) |
|