Sm2Co17磁体胞状组织边缘2:17R'相的透射电子显微镜表征 |
| 陈虹宇, 宋欣, 周相龙, 贾文涛, 袁涛, 马天宇 |
|
Identification of 2:17R' Cell Edge Phase in Sm2Co17-Type Permanent Magnets by Transmission Electron Microscopy |
| CHEN Hongyu, SONG Xin, ZHOU Xianglong, JIA Wentao, YUAN Tao, MA Tianyu |
| 图5 2:17R和2:17R'相的单胞、原子投影图和模拟的电子衍射花样 |
| Fig.5 Unit cells (a1, a2), projections (b1, d1, b2, d2), and simulated electron diffraction patterns (c1, e1, c2, e2) along [100]2:17R and [101]2:17R zone axes of 2:17R (a1-e1) and 2:17R' (a2-e2) |
|