表1 19种Fe-Co-Ni材料体系的组分信息
|
Table 1 Composition details of 19 Fe-Co-Ni alloys system
|
|
| Material | Designed mass | Analyzed mass | No. |
|---|
| system | ratio | fraction / % | | | Simple metal | Fe | Fe100.0 | 1 | | Fe-Ni | 6Fe-1Ni | Fe85.7Ni14.3 | 2 | | 3Fe-1Ni | Fe75.0Ni25.0 | 3 | | 1Fe-1Ni | Fe49.5Ni50.5 | 4 | | 1Fe-3Ni | Fe25.5Ni74.5 | 5 | | 1Fe-6Ni | Fe15.2Ni84.8 | 6 | | Simple metal | Ni | Ni100.0 | 7 | | Ni-Co | 6Ni-1Co | Ni84.3Co15.7 | 8 | | 3Ni-1Co | Ni75.6Co24.4 | 9 | | 1Ni-1Co | Ni51.6Co48.4 | 10 | | 1Ni-3Co | Ni25.4Co74.6 | 11 | | 1Ni-6Co | Ni15.0Co85.0 | 12 | | Simple metal | Co | Co100.0 | 13 | | Co-Fe | 6Co-1Fe | Co84.9Fe15.1 | 14 | | 3Co-1Fe | Co74.0Fe26.0 | 15 | | 1Co-1Fe | Co48.4Fe51.6 | 16 | | 1Co-3Fe | Co24.5Fe75.5 | 17 | | 1Co-6Fe | Co14.1Fe85.9 | 18 | | FeCoNi | 1Fe-1Co-1Ni | Fe33.8Co33.7Ni32.5 | 19 |
|
|
|