轴向超声振动对搅拌摩擦焊过程中金属流动行为的影响 |
| 何长树, 郄默繁, 张志强, 赵骧 |
|
Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding |
| HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang |
| 图8 FSW过程中SZ金属不同微区受力状态分析和金属流动示意图 (a) force condition of the plastic metal in the thread groove of pin (b) force condition of the plastic metal around the conical surface of pin (Fp1, Fp2—pressure forces; Ff1, Ff2—frictional forces; Fr1, Fr2—resultant forces) (c) schematic of plastic metal flow model in the SZ (ND—normal direction, TD—transverse direction, RD—rolling direction) |
| Fig.8 Schematics of force condition of different micro-zones and metal flow in SZ during FSW |
|