轴向超声振动对搅拌摩擦焊过程中金属流动行为的影响 |
| 何长树, 郄默繁, 张志强, 赵骧 |
|
Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding |
| HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang |
| 图6 距接头上表面5.2 mm处的SZ水平截面形貌的OM像 (a, c) FSW joint (b, d) UAFSW joint |