轴向超声振动对搅拌摩擦焊过程中金属流动行为的影响 |
| 何长树, 郄默繁, 张志强, 赵骧 |
|
Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding |
| HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang |
| 图4 距接头上表面0.2 mm处的搅拌区(SZ)水平截面形貌的OM像 (a) FSW joint (b) UAFSW joint |
| Fig.4 OM images of horizontal sections of the stir zone (SZ) at the distance of 0.2 mm from the top surface of the joints welded at rotation rate 1200 r/min and welding rate 160 mm/min |
|