恒电位脉冲技术对317L不锈钢点蚀行为及耐点蚀性能的影响 |
| 吕晨曦, 孙阳庭, 陈斌, 蒋益明, 李劲 |
|
Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel |
| LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin |
| 图7 PPT测试(Eh = 0.6 V)后与未经PPT测试317LSS样品的循环伏安曲线 |
| Fig.7 Cyclic voltammetry curves of 317LSS after PPT measurement (Eh = 0.6 V) and without PPT measurement |
|