恒电位脉冲技术对317L不锈钢点蚀行为及耐点蚀性能的影响 |
| 吕晨曦, 孙阳庭, 陈斌, 蒋益明, 李劲 |
|
Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel |
| LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin |
| 图5 不同高电位PPT测试后317LSS点蚀的尺寸分布 |
| Fig.5 Size distribution of pits of 317LSS after PPT test under Eh of 0.6 V, 0.8 V, and 1.0 V |
|