退火温度对含Nb高锰钢力学和阻尼性能的影响 |
| 王玉, 胡斌, 刘星毅, 张浩, 张灏云, 官志强, 罗海文 |
|
Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel |
| WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen |
| 图4 含Nb高锰钢不同温度退火后的阻尼性能和力学性能 (a) the relationship of logarithmic decrement (δ) and strain at the vibration of 1 Hz (b) engineering stress-strain curves of the specimens hot rolled and annealed at 750-1050oC (c) the relationship between logarithmic decrement of 0.1% strain amplitude and ultimate tensile strength |
| Fig.4 The damping and mechanical properties of Nb-contained high Mn steel |
|