退火温度对含Nb高锰钢力学和阻尼性能的影响 |
| 王玉, 胡斌, 刘星毅, 张浩, 张灏云, 官志强, 罗海文 |
|
Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel |
| WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen |
| 图2 热轧高锰钢在750~1050℃退火后组织的EBSD表征结果 (a-d) image quality (IQ) phase mapping (e-h) IPFs (i-l) grain reference orientation deviation (GROD) mapping |
| Fig.2 Microstructures characterized by EBSD when the hot rolled high Mn steel was annealed at the temperatures of 750-1050℃ |
|