SPS烧结参数对NiAl-28Cr-5.5Mo-0.5Zr合金微观组织及室温力学性能的影响 |
| 刘泽, 宁汉维, 林彰乾, 王东君 |
|
Influence of Spark Plasma Sintering Parameters on the Microstructure and Room-Temperature Mechanical Properties of NiAl-28Cr-5.5Mo-0.5Zr Alloy |
| LIU Ze, NING Hanwei, LIN Zhangqian, WANG Dongjun |
| 图6 不同时间烧结态NiAl基合金的微观组织 (a) 1 min (b) 3 min (c) 5 min (d) 7 min (e) 10 min (f) microcracks at the edge of specimen for t = 10 min |
| Fig.6 Microstructures of sintered NiAl-based alloy with different holding time at 1200oC |
|