CoCrFeNiCu高熵合金与304不锈钢真空扩散焊 |
| 李娟, 赵宏龙, 周念, 张英哲, 秦庆东, 苏向东 |
|
Diffusion Bonding of CoCrFeNiCu High-Entropy Alloy to 304 Stainless Steel |
| LI Juan, ZHAO Honglong, ZHOU Nian, ZHANG Yingzhe, QIN Qingdong, SU Xiangdong |
| 图2 CoCrFeNiCu HEA母材的OM像、XRD谱、SEM像和EDS结果 |
| Fig.2 OM (a) and SEM (c) images, XRD spectrum (b), and EDS result (d) of CoCrFeNiCu HEA base metal |
|