单晶高温合金共晶溶解行为的差热分析 |
| 张少华, 谢光, 董加胜, 楼琅洪 |
|
Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry |
| ZHANG Shaohua, XIE Guang, DONG Jiasheng, LOU Langhong |
| 图8 DD414单晶高温合金等温保温过程中的ln[-ln(1 - f(t))]-lnt曲线 |
| Fig.8 ln[-ln(1 - f(t))]-lnt curves of DD414 single crystal superalloy during isothermal holding process |
|