单晶高温合金共晶溶解行为的差热分析 |
| 张少华, 谢光, 董加胜, 楼琅洪 |
|
Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry |
| ZHANG Shaohua, XIE Guang, DONG Jiasheng, LOU Langhong |
| 图3 DD414单晶高温合金在1290℃保温不同时间的共晶形貌及分布图 |
| Fig.3 Morphologies (a-c) and distributions (eutectic colored by image software) (d-f) of the eutectics in DD414 single crystal superalloy after solution heat treatment at 1290℃ for 2 h (a, d), 6 h (b, e), and 10 h (c, f) |
|