单晶高温合金共晶溶解行为的差热分析 |
| 张少华, 谢光, 董加胜, 楼琅洪 |
|
Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry |
| ZHANG Shaohua, XIE Guang, DONG Jiasheng, LOU Langhong |
| 图2 DD414单晶高温合金铸态和热处理态组织(1310℃、6 h)的OM和SEM像 |
| Fig.2 OM (a, c) and SEM (b, d) images of the as-cast (a, b) and heat-treatment (1310oC, 6 h) (c, d) DD414 single crystal superalloy |
|