高温合金单晶铸件中共晶组织分布的表面效应 |
| 马德新, 赵运兴, 徐维台, 皮立波, 李重行 |
|
Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings |
| MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing |
| 图7 固溶热处理后的缘板与叶身转接处纵截面显微组织的OM像,及其两侧部位A和B的放大图 |
| Fig.7 OM images of longitudinal section microstructure at the junction between platform and aerofoil (b) and the magnifications showing the residual eutectics in areas A (a) and B (c) after solution heat treatment |
|