高温合金单晶铸件中共晶组织分布的表面效应 |
| 马德新, 赵运兴, 徐维台, 皮立波, 李重行 |
|
Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings |
| MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing |
| 图6 试棒侧表面区域横截面的铸态组织与固溶态组织的OM像 |
| Fig.6 OM images of transverse section near the sample surface showing the microstructures before (a) and after (b) solution heat treatment |
|