高温合金单晶铸件中共晶组织分布的表面效应 |
| 马德新, 赵运兴, 徐维台, 皮立波, 李重行 |
|
Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings |
| MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing |
| 图4 变截面试棒铸件的纵截面和横截面形貌,显示出环形上表面的共晶聚集现象 |
| Fig.4 Longitudinal section morphology of a bar sample with abrupt decrease in diameter (a) and the corresponding transverse section morphology (b), showing the eutectics accumulation on the ring-shaped upper surface |
|