高温合金单晶铸件中共晶组织分布的表面效应 |
| 马德新, 赵运兴, 徐维台, 皮立波, 李重行 |
|
Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings |
| MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing |
| 图3 单晶叶片缘板的纵截面及上、下表面的横截面显微组织的OM像 |
| Fig.3 OM images of longitudinal section microstructures of a blade platform (a) and transverse section near the upper (b) and bottom (c) surfaces |
|