低活化铁素体/马氏体钢组织调控及其固相连接研究进展 |
| 刘晨曦, 毛春亮, 崔雷, 周晓胜, 余黎明, 刘永长 |
|
Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels |
| LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang |
| 图15 RAFM钢搅拌摩擦焊(FSW)接头临界热影响区中Laves相的TEM明场相、高角环形暗场像和能谱图[ (a) bright field TEM image (b) HAADF scanning image (c-f) EDX maps |
| Fig.15 Laves phase in intercritical heat affect zone of friction stir welding (FSW) of a RAFM steel[ |
|