低活化铁素体/马氏体钢组织调控及其固相连接研究进展 |
| 刘晨曦, 毛春亮, 崔雷, 周晓胜, 余黎明, 刘永长 |
|
Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels |
| LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang |
| 图7 RAFM钢的拉伸强度、屈服强度及延伸率随温度的变化[ |
| Fig.7 Tensile stress, yield stress, and total elongation of a RAFM steel as a function of temperature[ |
|