低活化铁素体/马氏体钢组织调控及其固相连接研究进展 |
| 刘晨曦, 毛春亮, 崔雷, 周晓胜, 余黎明, 刘永长 |
|
Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels |
| LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang |
| 图6 不同热处理状态下RAFM钢的室温屈服强度实测值与计算值对比[ |
| Fig.6 Comparisons between the experimental and calculated yield strengths at room temperature of a RAFM steel under the different heat treatments (N&T 1—normalzing at 1000oC for 30 min and tempering at 750oC for 90 min, N&T 2—normalzing at 1050oC for 30 min and tempering at 750oC for 90 min)[ |
|