低活化铁素体/马氏体钢组织调控及其固相连接研究进展 |
| 刘晨曦, 毛春亮, 崔雷, 周晓胜, 余黎明, 刘永长 |
|
Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels |
| LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang |
| 图4 含0.1%C的RAFM钢5℃/min冷却时不同阶段的激光共聚焦显微镜照片与马氏体相变曲线 |
| Fig.4 Images of laser scanning confocal microscopy in the RAFM steel containing 0.1%C and the corresponding martensitic transformation curve with a cooling rate of 5oC/min applied |
|