增材制造可降解金属医用植入物 |
郑玉峰, 夏丹丹, 谌雨农, 刘云松, 徐钰倩, 温鹏, 田耘, 赖毓霄 |
Additively Manufactured Biodegrabable Metal Implants |
ZHENG Yufeng, XIA Dandan, SHEN Yunong, LIU Yunsong, XU Yuqian, WEN Peng, TIAN Yun, LAI Yuxiao |
图4 AM多孔生物材料单元体结构总结[ (a) beam-based designs[ (b) topological design based on four different types of triply periodic minimal surfaces (TPMS)[ (c) a catalogue of different types of minimal surfaces[ |
Fig.4 The summary of additively manufactured porous biomaterials' lattice structures |
![]() |