增材制造可降解金属医用植入物 |
| 郑玉峰, 夏丹丹, 谌雨农, 刘云松, 徐钰倩, 温鹏, 田耘, 赖毓霄 |
|
Additively Manufactured Biodegrabable Metal Implants |
| ZHENG Yufeng, XIA Dandan, SHEN Yunong, LIU Yunsong, XU Yuqian, WEN Peng, TIAN Yun, LAI Yuxiao |
| 图3 L-PBF成形WE43的激光功率-扫描速率窗口图[ |
| Fig.3 Power-speed process map for L-PBF prepared WE43 (a)[ |
|